Study of the reactions between iron ore slag and refractories
For the fabrication of iron ore pellets at LKAB (Luossavaara-Kiirunavaara AB), one of the methods used is to sinter the pellets in a rotary kiln. This Kiln has a drift temperature of 1250°C in average. During this process a coating, causing the